I need some TIG advice please

So as u have seen on the pictures I just can't figure out what I am doing wrong that these welds Keep getting like some sort of Slack?

(I've only started welding about 2-3 days ago it's just a Hobby)

Im running a 2,4mm Tungsten elektrode on about 100 Amps and it's a Lift TIG (the Nozzle is a 5 and im running on ~6l per min)

Is it not cleaned enough? I cleaned the inside but not the full Outside.

Thanks in Advance