Hey everyone, a couple of weeks ago I posted my thermals asking about a re-paste due to excessive hotspot temp (113c). Just finished completing it using PTM7950 and well, look at the difference! I included a before and after. Also a couple pics of the die included for fun - you can see the paste pump-out on the die and heat sink. Overall the procedure itself wasn't too difficult - just nerve wracking due to market conditions. I ended up re-using the pads due to how clean they were. These results were also just after application, I have not let the PTM7950 "settle" yet so the temps should get even better.